Skip to page content
USDA Forest Service
  
Treesearch

Research & Development Treesearch

 
Treesearch Home
About Treesearch
Contact Us
Research & Development
Forest Products Lab
International Institute of Tropical Forestry
Northern
Pacific Northwest
Pacific Southwest
Rocky Mountain
Southern Research Station
Help
 

Science.gov - We Participate


USA.gov  Government Made Easy


Global Forest Information Service

US Forest Service
P.O. Box 96090
Washington, D.C.
20090-6090

(202) 205-8333

You are here: Home / Search / Publication Information
Bookmark and Share

Publication Information

View PDF (1.9 MB bytes)

Title: Durability of structural lumber products after exposure at 82°C and 80% relative humidity

Author: Green, David W.; Evans, James W.; Hatfield, Cherilyn A.; Byrd, Pamela J.;

Date: 2005

Source: Research Paper FPL-RP-631. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 21 p.

Publication Series: Research Paper (RP)

Description: Solid-sawn lumber (Douglas-fir, southern pine, Spruce–Pine–Fir, and yellow-poplar), laminated veneer lumber (Douglas-fir, southern pine, and yellow-poplar), and laminated strand lumber (aspen and yellow-poplar) were heated continuously at 82°C (180°F) and 80% relative humidity (RH) for periods of up to 24 months. The lumber was then reconditioned to room temperature at 20% RH and tested in edgewise bending. Little reduction occurred in modulus of elasticity (MOE) of solid-sawn lumber, but MOE of composite lumber products was somewhat reduced. Modulus of rupture (MOR) of solid- sawn lumber was reduced by up to 50% after 24 months exposure. Reductions in MOR of up to 61% were found for laminated veneer lumber and laminated strand lumber after 12 months exposure. A limited scope study indicated that the results for laminated veneer lumber in edgewise bending are also applicable to flatwise bending. Comparison with previous results at 82°C(180°F)/25% RH and at 66°C (150°F)/20% RH indicate that differences in the permanent effect of temperature on MOR between species of solid-sawn lumber and between solid-sawn lumber and composite lumber products are greater at high humidity levels than at low humidity levels. This report also describes the experimental design of a program to evaluate the permanent effect of temperature on flexural properties of structural lumber, with reference to previous publications on the immediate effect of temperature and the effect of moisture content on lumber properties.

Keywords: Lumber, laminated veneer lumber, laminated strand lumber, modulus of rupture, modulus of elasticity, long-term temperature exposure

Publication Notes:

  • We recommend that you also print this page and attach it to the printout of the article, to retain the full citation information.
  • This article was written and prepared by U.S. Government employees on official time, and is therefore in the public domain.

XML: View XML

Citation:


Green, David W.; Evans, James W.; Hatfield, Cherilyn A.; Byrd, Pamela J. 2005. Durability of structural lumber products after exposure at 82°C and 80% relative humidity. Research Paper FPL-RP-631. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 21 p.

 