Skip to page content
USDA Forest Service
  
Treesearch

Research & Development Treesearch

 
Treesearch Home
About Treesearch
Contact Us
Research & Development
Forest Products Lab
International Institute of Tropical Forestry
Northern
Pacific Northwest
Pacific Southwest
Rocky Mountain
Southern Research Station
Help
 

Science.gov - We Participate


USA.gov  Government Made Easy


Global Forest Information Service

US Forest Service
P.O. Box 96090
Washington, D.C.
20090-6090

(202) 205-8333

You are here: Home / Search / Publication Information
Bookmark and Share

Publication Information

View PDF (631 KB bytes)

Title: Fire resistance of wood members with directly applied protection

Author: White, Robert H.;

Date: 2009

Source: Fire and materials, 2009 [electronic resource] : 11th International Conference and Exhibition, 26-28, January 2009, Fisherman's Wharf, San Francisco, USA. London : Interscience Communications Ltd., 2009: [12] pages.

Publication Series: Miscellaneous Publication

Description: Fire-resistive wood construction is achieved either by having the structural elements be part of fire-rated assemblies or by using elements of sufficient size that the elements themselves have the required fire-resistance ratings. For exposed structural wood elements, the ratings in the United States are calculated using either the T.T. Lie method or the National Design Specifications (NDS) Method. There is no widely accepted methodology in the United States to determine the fire-resistance rating of an individual structural wood element with the protective membrane directly applied to the exposed surfaces of the element. In these tests, we directly applied one or two layers of 16-mm thick fire-rated gypsum board or 13-mm thick southern pine plywood for the protective membrane to the wood element. The wood elements were Douglas-fir laminated veneer lumber (LVL) specimens and Douglas-fir glued-laminated specimens that had previously been tested without any protective membrane. The methodology for the tension testing in the horizontal furnace was the same used in the earlier tests. The fire exposure was ASTM E 119. For the seven single-layer gypsum board specimens, the improvements ranged from 25 to 40 min. with an average value of 33 min. For the three double-layer specimens, the improvement in times ranged from 64 to 79 min. with an average value of 72 min. We concluded that times of 30 min. for a single layer of 16-mm Type X gypsum board and at least 60 min. for a double layer of 16-mm Type X gypsum board can be added to the fire rating of an unprotected structural wood element to obtain the rating of the protected element.

Keywords: Veneers, gypsum, Douglas fir, plywood, fire testing, laminated wood, testing, thermal properties, fireproofing agents, fireproofing of wood, flammability, fire resistance, failure, tension, gypsum board, Southern pine, glulam timbers, ASTM E 119, fire hazard, fire resistance, thermal degradation

Publication Notes:

  • We recommend that you also print this page and attach it to the printout of the article, to retain the full citation information.
  • This article was written and prepared by U.S. Government employees on official time, and is therefore in the public domain.

XML: View XML

Citation:


White, Robert H. 2009. Fire resistance of wood members with directly applied protection. Fire and materials, 2009 [electronic resource] : 11th International Conference and Exhibition, 2009 January 26-28, Fisherman''s Wharf, San Francisco, USA. London: Interscience Communications Ltd.: 492-503.

 