Skip to page content
USDA Forest Service
  
Treesearch

Research & Development Treesearch

 
Treesearch Home
About Treesearch
Contact Us
Research & Development
Forest Products Lab
International Institute of Tropical Forestry
Northern
Pacific Northwest
Pacific Southwest
Rocky Mountain
Southern Research Station
Help
 

Science.gov - We Participate


USA.gov  Government Made Easy


Global Forest Information Service

US Forest Service
P.O. Box 96090
Washington, D.C.
20090-6090

(202) 205-8333

You are here: Home / Search / Publication Information
Bookmark and Share

Publication Information

View PDF (599.0 KB bytes)

Title: Wood Products Thermal Degradation and Fire

Author: Dietenberger, Mark; Hasburgh, Laura;

Date: 2016

Source: Reference Module in Materials Science and Materials Engineering

Publication Series: Scientific Journal (JRNL)

Description: As wood reaches elevated temperatures, the different chemical components undergo thermal degradation that affect the performance of wood. The extent of these changes depends on the temperature level and length of time under exposure conditions. Permanent reductions in strength and modulus of elasticity can occur at temperatures >65 °C, with the amount depending on the temperature, pH of wood, moisture content, heating medium, exposure period, chemical treatment, and species (Winandy and Rowell, 2013). Studies relating strength reduction with temperature rise has indicated a kinetic basis(involving activation energy, pre-exponential factor, and order of reaction). If the specimens are tested while still hot after long term exposure (∼66 °C for 3 years), the percentage of strength reduction would be based on the combination of an immediate effect of temperature (∼14%) and a permanent effect (∼33%) for a total of around 47% strength loss (Green and Evans, 2008). The primary mechanism for this degradation is the production of acetic acid freed by the process of hydrolysis at long term ambient conditions that include varying moisture contents and by which the acetyl groups are split from their association with hemicelluloses in the wood (Packman, 1960). During hydrothermal treatments (as reported for up to 230 °C), the acetyl groups present in wood hemicelluloses hydrolyze to form acetic acid which provides the hydronium ions needed to self-catalyze the hydrolysis of wood, involving the hydrolytic reactions of ether and ester bonds (Garrote et al., 2002). Long term exposure to temperatures equal to or greater than 66 °C is not a concern in residential construction but may be an important consideration for certain industrial buildings. However, strength and stiffness degradation relationships with temperatures greater than 66 °C and varying time durations for wood under compression and tension has recently been utilized in building design for fire protection (Eurocode 5, 2004).

Keywords: Wood products: aging of wood, Wood products: chemical degradation, Wood: strength and stiffness, Wood: thermal properties

Publication Notes:

  • We recommend that you also print this page and attach it to the printout of the article, to retain the full citation information.
  • This article was written and prepared by U.S. Government employees on official time, and is therefore in the public domain.

XML: View XML

Citation:


Dietenberger, M.A.; Hasburgh, L.E. 2016. Wood products thermal degradation and fire. Reference Module in Materials Science and Materials Engineering. 8 pp.

 